Maywogreen ABS PCR consists of PCR-materials. Post-consumer recycled materials are materials that are generated in households, public, commercial and industrial facilities after their use phase and can no longer be used for their intended purpose.

| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Density | DIN EN ISO 1183-1 | g / cm3 | 1,07 |
| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Yield stress | DIN EN ISO 527 | MPa | 40 |
| Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 2200 |
| Notched impact strength | DIN EN ISO 179 | kJ / m2 | 8 |
| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | °C | > 180 °C |
| Vicat softening temperature | DIN EN ISO 306, Vicat B | °C | 90 |
| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Surface resisitivity | DIN EN 61340 | Ω | > 1012 |
| Volume resistivity | DIN EN 61340 | Ω | > 1012 |