| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Density | DIN EN ISO 1183-1 | g / cm3 | 0,95 |
| Water absorption | DIN EN ISO 62 | % | 0,01 |
| Flammability (Thickness 3 mm / 6 mm) | UL 94 | HB | |
| Melt Flow Rate (MFR 190/5) | DIN EN ISO 1133 | g / 10 min | Kein fließen |
| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Yield stress | DIN EN ISO 527 | MPa | 24 |
| Elongation at break | DIN EN ISO 527 | % | >250 |
| Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 1100 |
| Notched impact strength | DIN EN ISO 11542-2 | kJ / m2 | 40 |
| Shore hardness | DIN EN ISO 868 | scale D | 63 |
| Test Method | Unit | Guideline Value | |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | °C | 130 ... 135 |
| Coefficient of linear thermal expansion | DIN 53752 | 10-6 / K | 150 ... 230 |
| Service temperature, long term | Average | °C | -100 … 80 |
| Service temperature, short term (max.) | Average | °C | 80 |
| Vicat softening temperature | DIN EN ISO 306, Vicat B | °C | 79 |