SKU | Name | Type | Type | Color | Measurements | Length | Width | Thickness | Height | ||
---|---|---|---|---|---|---|---|---|---|---|---|
No stock item (MOQ) | 298740 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | bright red orange, similar RAL 2008 | 2.440 x 1.220 x 19 mm | 2,440 mm | 1,220 mm | 19 mm | ||
No stock item (MOQ) | 333251 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | bright red orange, similar RAL 2008 | 3.000 x 1.500 x 20 mm | 3,000 mm | 1,500 mm | 20 mm | ||
No stock item (MOQ) | 337700 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | deep orange, similar RAL 2011 | 2.440 x 1.500 x 19 mm | 2,440 mm | 1,500 mm | 19 mm | ||
No stock item (MOQ) | 370032 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | orange | 2.440 x 1.220 x 19 mm | 2,440 mm | 1,220 mm | 19 mm | ||
No stock item (MOQ) | 373890 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | orange | 2.440 x 1.220 x 19 mm | 2,440 mm | 1,220 mm | 19 mm | ||
Stock item (no MOQ) | 450271 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | bright red orange, similar RAL 2008 | 3.000 x 1.500 x 19 mm | 3,000 mm | 1,500 mm | 19 mm | ||
No stock item (MOQ) | 475752 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | pure orange, similar RAL 2004 | 3.000 x 1.500 x 15 mm | 3,000 mm | 1,500 mm | 15 mm | ||
No stock item (MOQ) | 475759 | Play-Tec® UV-stabilized orange extruded | sheet | sheet | pure orange, similar RAL 2004 | 3.000 x 1.500 x 19 mm | 3,000 mm | 1,500 mm | 19 mm |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | DIN EN ISO 1183-1 | g / cm3 | >0,91 |
Water absorption | DIN EN ISO 62 | % | 0,1 |
Flammability (Thickness 3 mm / 6 mm) | UL 94 | HB |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Yield stress | DIN EN ISO 527 | MPa | >23 |
Elongation at break | DIN EN ISO 527 | % | >50 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | >1100 |
Notched impact strength | DIN EN ISO 179 | kJ / m2 | >30 |
Shore hardness | DIN EN ISO 868 | scale D | >65 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Melting temperature | ISO 11357-3 | °C | 162 ... 165 |
Thermal conductivity | DIN 52612-1 | W / (m * K) | 0,20 |
Thermal capacity | DIN 52612 | kJ / (kg * K) | 1,70 |
Coefficient of linear thermal expansion | DIN 53752 | 10-6 / K | 120 ... 190 |
Service temperature, long term | Average | °C | -30 … 100 |
Service temperature, short term (max.) | Average | °C | 150 |
Vicat softening temperature | DIN EN ISO 306, Vicat B | °C | 85 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Dielectric constant | IEC 60250 | 2,5 | |
Dielectric dissipation factor (106 Hz) | IEC 60250 | 0,00019 | |
Volume resistivity | DIN EN 62631-3-1 | Ω * cm | >1014 |
Surface resistivity | DIN EN 62631-3-2 | Ω | >1014 |
Comparative tracking index | IEC 60112 | 600 | |